I’m sure someone is going to dispute this, live and learn!
You are correct!
I’m totally disputing this. Since the ideal material for storing acids is glass, and highly corrosive hydrofluoric acid is about the only acid that etches glass, this is pegging my Poppycock meter to the point I had to unplug it and take an aspirin. Some manufactures literally acid etched their date codes on their tubes without stressing the integrity of the glass after decades. 🤔